The Resource Static tensile and tensile creep testing of four boron nitride coated ceramic fibers at elevated temperatures : final report, Scott L. Coguill, Donald F. Adams, Richard S. Zimmerman, (microform)

Static tensile and tensile creep testing of four boron nitride coated ceramic fibers at elevated temperatures : final report, Scott L. Coguill, Donald F. Adams, Richard S. Zimmerman, (microform)

Label
Static tensile and tensile creep testing of four boron nitride coated ceramic fibers at elevated temperatures : final report
Title
Static tensile and tensile creep testing of four boron nitride coated ceramic fibers at elevated temperatures
Title remainder
final report
Statement of responsibility
Scott L. Coguill, Donald F. Adams, Richard S. Zimmerman
Creator
Contributor
Subject
Language
eng
Member of
Additional physical form
Also available via Internet from the NTRS web site. Address as of 2/23/05: http://ntrs.nasa.gov/archive/nasa/casi.ntrs.nasa.gov/19900002491%5F1990002491.pdf; current access is available via PURL.
Cataloging source
GPO
http://library.link/vocab/creatorName
Coguill, Scott L
Government publication
federal national government publication
Index
no index present
Literary form
non fiction
Nature of contents
bibliography
http://library.link/vocab/relatedWorkOrContributorName
  • Adams, Donald F
  • Zimmerman, Richard S
  • Ames Research Center
Series statement
NASA contractor report
Series volume
184999
http://library.link/vocab/subjectName
  • Boron nitrides
  • Ceramic fibers
  • High temperature tests
  • Static tests
  • Tensile creep
  • Tensile tests
Label
Static tensile and tensile creep testing of four boron nitride coated ceramic fibers at elevated temperatures : final report, Scott L. Coguill, Donald F. Adams, Richard S. Zimmerman, (microform)
Link
http://purl.access.gpo.gov/GPO/LPS58255
Instantiates
Publication
Note
  • "August 1989."
  • "NASA grant no. NAG-2-470."
Bibliography note
Includes bibliographical references
Extent
1 v.
Form of item
microfiche
Reproduction note
Microfiche.
Stock number
N 90-11807
System control number
  • 2413696-01okla_normanlaw
  • (SIRSI)2413696
  • (Sirsi) o57715447
  • (GPO)99164721
  • (OCoLC)57715447
Label
Static tensile and tensile creep testing of four boron nitride coated ceramic fibers at elevated temperatures : final report, Scott L. Coguill, Donald F. Adams, Richard S. Zimmerman, (microform)
Link
http://purl.access.gpo.gov/GPO/LPS58255
Publication
Note
  • "August 1989."
  • "NASA grant no. NAG-2-470."
Bibliography note
Includes bibliographical references
Extent
1 v.
Form of item
microfiche
Reproduction note
Microfiche.
Stock number
N 90-11807
System control number
  • 2413696-01okla_normanlaw
  • (SIRSI)2413696
  • (Sirsi) o57715447
  • (GPO)99164721
  • (OCoLC)57715447

Library Locations

  • Architecture LibraryBorrow it
    Gould Hall 830 Van Vleet Oval Rm. 105, Norman, OK, 73019, US
    35.205706 -97.445050
  • Bizzell Memorial LibraryBorrow it
    401 W. Brooks St., Norman, OK, 73019, US
    35.207487 -97.447906
  • Boorstin CollectionBorrow it
    401 W. Brooks St., Norman, OK, 73019, US
    35.207487 -97.447906
  • Chinese Literature Translation ArchiveBorrow it
    401 W. Brooks St., RM 414, Norman, OK, 73019, US
    35.207487 -97.447906
  • Engineering LibraryBorrow it
    Felgar Hall 865 Asp Avenue, Rm. 222, Norman, OK, 73019, US
    35.205706 -97.445050
  • Fine Arts LibraryBorrow it
    Catlett Music Center 500 West Boyd Street, Rm. 20, Norman, OK, 73019, US
    35.210371 -97.448244
  • Harry W. Bass Business History CollectionBorrow it
    401 W. Brooks St., Rm. 521NW, Norman, OK, 73019, US
    35.207487 -97.447906
  • History of Science CollectionsBorrow it
    401 W. Brooks St., Rm. 521NW, Norman, OK, 73019, US
    35.207487 -97.447906
  • John and Mary Nichols Rare Books and Special CollectionsBorrow it
    401 W. Brooks St., Rm. 509NW, Norman, OK, 73019, US
    35.207487 -97.447906
  • Library Service CenterBorrow it
    2601 Technology Place, Norman, OK, 73019, US
    35.185561 -97.398361
  • Price College Digital LibraryBorrow it
    Adams Hall 102 307 West Brooks St., Norman, OK, 73019, US
    35.210371 -97.448244
  • Western History CollectionsBorrow it
    Monnet Hall 630 Parrington Oval, Rm. 300, Norman, OK, 73019, US
    35.209584 -97.445414
Processing Feedback ...